广州领拓仪器科技有限公司
广州领拓仪器科技有限公司

Silicon carbide ( SiC nano particles)粒度分析报告

2015-01-29476
行业应用: 建材/家具 家具

文件大小:452.06KB

建议WIFI下载,土豪忽略

方案优势
We recommend a dispersing time of minimum 30min in the ultrasonic bath LABORETTE 17!Measurement:ANALYSETTE 22 NanoTec plus with Wet Dispersion Unit.Sample preparation:dispersing in diluted tensid + 0,1% Na4P2O7 and 30min ultrasonic duration with LABORETTE 17. Dispersion:Wet in water Theory: Mie Theory Comments:we recommend a dispersing time of minimum 30min in the ultrasonic bath LABORETTE 17!
相关产品

网站导航