奥码拓(北京)科技有限公司
奥码拓(北京)科技有限公司

A practical methodology to select fretting palliativ

2011-06-01372
行业应用: 环保/水工业 环境水

文件大小:577.04KB

建议WIFI下载,土豪忽略

方案优势
Abstract Considered as a plague for numerous industrial assemblies, fretting, associated to slight oscillatory displacement, is encountered in all quasi-static contacts subjected to vibration. Depending on sliding conditions, cracking or wear damage can be observed. During the past three decades there has been a huge development in surface treatments. Thousands of new surface treatments and coatings are now available. The critical challenge is to evaluate such treatments against fretting loadings. To achieve this objective, a fast fretting methodology has been developed. It consists in quantifying the palliative friction, cracking and wear responses through a very small number of fretting tests. By defining quantitative variables, a normalized polar fretting damage chart approach is introduced. Applied to shot peening, chromium coatings and WC-Co coatings, it demonstrates the potential benefit of a thermal sprayed WC-Co coating. © 2005 Elsevier B.V. All rights reserved. DN 55 1200度高温微动/滑动/冲击摩擦试验机
相关产品

网站导航